Maximum Metal Thickness to be Punched
|
|
Hot Rolled C-1095 Annealed = 0.31 Mild A-7 = 0.5 Boiler Plate = 0.5 Struct Corten (ASTM A242) = 0.44 Hot Rolled C-1095 = 0.25 Structural A-36 = 0.5 Cold Rolled C-1018 = 0.5 Hot Rolled C1050 = 0.4 Stainless Annealed = 0.4 Stainless 304 Hot Rolled = 0.4 Stainless 316 Cold Rolled = 0.4
|