Maximum Metal Thickness to be Punched
|
|
Mild A-7 = 0.31 Boiler Plate = 0.31 Structural A-36 = 0.25 Struct Corten (ASTM A242) = 0.25 Cold Rolled C-1018 = 0.25 Hot Rolled C1050 = 0.25 Hot Rolled C-1095 = 0.13 Hot Rolled C-1095 Annealed = 0.19 Stainless Annealed = 0.25 Stainless 304 Hot Rolled = 0.25 Stainless 316 Cold Rolled = 0.25
|